dc.description.abstract | En la actualidad los minerales de oro son comúnmente procesados mediante técnicas de lixiviación que utilizan como agente lixiviante al cianuro; sin embargo en la última década el uso del cianuro, ha sido restringido, por su carácter tóxico que lo hace nocivo para el ser humano y la vida silvestre. Es por esto que se han investigado agentes lixiviantes diferentes al cianuro, con el fin de utilizarlos como alternativas en los procesos de lixiviación de oro, entre los que se destaca la tiourea. En el presente trabajo se estudiaron dos minerales de diferente naturaleza auroargentíferos Santandereanos: sulfurado y oxidado. Se determinó la refractariedad, composición química y mineralógica de cada uno con el fin de describir la naturaleza de éstos y estudiar la respuesta de los procesos de lixiviación con cianuro y tiourea con base en su composición. De igual manera, se estudiaron y compararon las eficiencias de disolución de oro y plata para estos dos tipos de minerales con ambos métodos de lixiviación. Las mejores condiciones de operación de la lixiviación con tiourea (6 g/L CS(NH2)2, relación molar Fe2(SO4)3/ CS(NH2)2 de 1/2 y potencial redox de 510 mV/SHE) fueron halladas al estudiar por separado las variables de concentración de tiourea, relación molar Fe2(SO4)3/ CS(NH2)2 y potencial redox. El mineral oxidado, presentó una máxima disolución de oro de 94% y de plata de 23% para un tiempo de lixiviación con tiourea de 10 horas, mientras que para un periodo de 35 horas de lixiviación con cianuro se alcanzó una disolución de 88% de oro y 87% de plata. Por su parte, el mineral sulfurado presentó una disolución de oro de 97% y de plata de 23% para la lixiviación con tiourea, mientras que para la lixiviación con cianuro se alcanzó una disolución de tan solo el 46% de oro y 12.1% de plata. Concluyéndose que el proceso de lixiviación con tiourea para extraer oro resulta factible comparada con el cianuro, pero su costo elevado de operación debido a altos consumos de tiourea limitan la aplicación del proceso a nivel industrial. | |
dc.description.abstractenglish | Nowadays the gold mineral is processed through leaching technical that use cyanide leaching agents; however during the last decade the use of cyanide has been restricted, for its toxic character that makes it harmful to humans and wildlife. For this reason it has investigated different cyanide leaching agents, with the purpose of using it as alternative in gold leaching process, among which stand up the thiourea. In this research report two minerals have been studied of different auriferous nature Santandereanos: sulphurated and oxidized. The refractoriness was determined, chemical composition and each mineralogical with the purpose of describe the nature of them and study the response of the processes of leaching with cyanide and thiourea based in them composition. Similarly, was studied and compared the dilution efficiencies of the gold and silver for these two kin of mineral with both leaching methods. The best operate conditions of the leaching with thiourea (6 g/L CS(NH2)2, molar relaxation Fe2(SO4)3/CS(NH2)2 of 1/2 and redox potential 510 mV/SHE) were found out when studying for separate the concentration variables of thiourea, molar relaxation Fe2(SO4)3/CS(NH2)2 and redox potential. Regarding, oxidized mineral, it presented a gold dilution máxima of 94% and silver of 23% for a time of leaching with thiourea of 10 hours, while for leaching with cyanide the gold dilution reached 88% and silver 87% in 35 hours. Moreover, the gold mineral sulphurated dilution presented 97% and silver 23% for leaching with thiourea, whereas for the leaching with cyanide the dilution reached 46% of gold and 12.1% of silver. Finally Concludes, the leaching processes with thiourea for gold extraction feasible compared with cyanide, but its high cost of operation due to high consumption of thiourea, this limit the application in industrial processes. | |
dc.description.degreelevel | Pregrado | |
dc.description.degreename | Ingeniero Metalúrgico | |
dc.format.mimetype | application/pdf | |
dc.identifier.instname | Universidad Industrial de Santander | |
dc.identifier.reponame | Universidad Industrial de Santander | |
dc.identifier.repourl | https://noesis.uis.edu.co | |
dc.identifier.uri | https://noesis.uis.edu.co/handle/20.500.14071/28517 | |
dc.language.iso | spa | |
dc.publisher | Universidad Industrial de Santander | |
dc.publisher.faculty | Facultad de Ingenierías Fisicoquímicas | |
dc.publisher.program | Ingeniería Metalúrgica | |
dc.publisher.school | Escuela de Ingeniería Metalúrgica y Ciencia de Materiales | |
dc.rights | http://creativecommons.org/licenses/by/4.0/ | |
dc.rights.accessrights | info:eu-repo/semantics/openAccess | |
dc.rights.creativecommons | Atribución-NoComercial-SinDerivadas 4.0 Internacional (CC BY-NC-ND 4.0) | |
dc.rights.license | Attribution-NonCommercial 4.0 International (CC BY-NC 4.0) | |
dc.rights.uri | http://creativecommons.org/licenses/by-nc/4.0 | |
dc.subject | Tiourea | |
dc.subject | Cianuración | |
dc.subject | Lixiviación De Oro Y Plata | |
dc.subject | Refractariedad De Los Minerales. | |
dc.subject.keyword | Thiourea | |
dc.subject.keyword | Cyanidation | |
dc.subject.keyword | Gold And Silver Leaching | |
dc.subject.keyword | Refractory Minerals. | |
dc.title | Estudio comparativo de la lixiviación de dos minerales auroargentiferos (oxidado y sulfurado) con cianuro y tiourea | |
dc.title.english | Comparative study of the leaching of two auriferous minerals (oxidized and sulphurated) with cyanide and thiourea. | |
dc.type.coar | http://purl.org/coar/version/c_b1a7d7d4d402bcce | |
dc.type.hasversion | http://purl.org/coar/resource_type/c_7a1f | |
dc.type.local | Tesis/Trabajo de grado - Monografía - Pregrado |
Files
Original bundle
1 - 3 of 3
No Thumbnail Available
- Name:
- Carta de autorización.pdf
- Size:
- 463.02 KB
- Format:
- Adobe Portable Document Format
No Thumbnail Available
- Name:
- Nota de proyecto.pdf
- Size:
- 44.65 KB
- Format:
- Adobe Portable Document Format