Concentración de arenas negras provenientes de Barbacoas (Nariño) y evaluación de su procesamiento por molienda de alta energía para la obtención de ilmenita de tamaño nanométrico
dc.contributor.advisor | Pedraza Rosas, Julio Elias | |
dc.contributor.advisor | Pedraza Avella, Julio Andrés | |
dc.contributor.advisor | Albarracin Arias, Jorge Alberto | |
dc.contributor.author | Arias Gonzalez, Andres Felipe | |
dc.contributor.author | Celis Barrera, Hernan Daniel | |
dc.date.accessioned | 2024-03-03T23:14:43Z | |
dc.date.available | 2017 | |
dc.date.available | 2024-03-03T23:14:43Z | |
dc.date.created | 2017 | |
dc.date.issued | 2017 | |
dc.description.abstract | En diversos yacimientos de minerales en Colombia se pueden encontrar depósitos de arenas negras, que contienen minerales de gran importancia por sus aplicaciones, como es el caso de la ilmenita. Se determinó un circuito de concentración para la extracción de ilmenita de un depósito de arenas negras de Barbacoas(Nariño, Colombia), fueron evaluados concentradores gravimétricos; una espiral concentradora teniendo en cuenta el tiempo de operación(3-5min) y la concentración de sólidos en pulpa(10-20%) y una mesa vibratoria Wilfley(0,6L/s,11º); separadores magnéticos, uno de alta intensidad de campo magnético en húmedo(WHIMS), variando la intensidad del campo magnético(5-20%) y otro de baja intensidad de campo en seco(DLIMS). El circuito seleccionado comienza con la espiral durante 5 minutos de operación y una concentración de solidos del 10%, cuyos concentrados pasan al separador magnético en húmedo con una intensidad de campo magnético del 5%(400 Gauss) obteniendo los mejores resultados en ley de ilmenita y fracción de concentrado (92,78% y 0,76 respectivamente). La composición elemental de las arenas negras fue analizada mediante FRX, para determinar las fases cristalinas que componen las arenas y sus concentrados se caracterizaron a través de DRX; la morfología y aspecto fueron analizados por medio de microscopía óptica. Los concentrados con alta ley de ilmenita, se sometieron a un proceso de molienda de alta energía en un molino Atrritor(948cm3), evaluando la obtención del tamaño en escala nanométrica (fracción de distribución de tamaño(<100nm), teniendo en cuenta variables como: el tiempo de operación, la relación másica bolas:mineral(50:1 o 100:1), la frecuencia del molino(400-600 rpm), el diámetro de bolas(3-4,8mm). La distribución del tamaño de partícula de los concentrados molidos fue determinada mediante microscopía óptica y dispersión dinámica de la luz(DLS). Las mejores condiciones de molienda fueron: relación 50:1, frecuencia de 600 rpm, diámetro de bolas de 4,8 mm y un tiempo de operación de 3 horas. | |
dc.description.abstractenglish | In various mineral deposits in Colombia can be found black sands deposits, which contain minerals of great importance for their applications, such as is the case of the ilmenite. Gravimetric concentrators, a concentrator spiral taking into account the operating time(3-5 min) and pulp concentration (10-20%) and a Wilfley vibratory table (0,6 L/s, 11º); magnetic separators, a wet high intensity magnetic separator (WHIMS), varying the intensity of the magnetic field (5-20%), and a dry low intensity magnetic separator (DLIMS) were evaluated to define a concentration circuit for the extraction of ilmenite, from a black sands deposit in Barbacoas (Nariño, Colombia). The selected circuit starts with a spiral during 5 minutes of operation and a solids concentration of 10%, whose concentrates are carried to a wet high intensity magnetic separator with a field intensity of 5% (400 Gauss); getting the best results in fineness and recovery percentage of ilmenite (92,78% and 0,76 respectly). The elemental composition of the black sands was analized by FRX, the crystalline phases that compose the sands and their concentrates, were characterized by XRD, its morphology and appearance were analyzed by optical microscopy. Concentrates with high ilmenite fineness were subjected to a high energy milling in an Atrritor mill (948 cm3), evaluating the size at nanoscale (size distribution fraction <100 nm), and considering variables such as: operating time, mass ratio balls: mineral (50: 1 or 100: 1), mill frequency (400 or 600 rpm) and ball diameter (3-4.8 mm). The particle size distribution of milled concentrates was determined by optical microscopy and dynamic light scattering (DLS). The best milling conditions were: 50:1 ratio, 600 rpm frequency, 4.8 mm ball diameter and an operating time of 3 hours. | |
dc.description.degreelevel | Pregrado | |
dc.description.degreename | Ingeniero Químico | |
dc.format.mimetype | application/pdf | |
dc.identifier.instname | Universidad Industrial de Santander | |
dc.identifier.reponame | Universidad Industrial de Santander | |
dc.identifier.repourl | https://noesis.uis.edu.co | |
dc.identifier.uri | https://noesis.uis.edu.co/handle/20.500.14071/35826 | |
dc.language.iso | spa | |
dc.publisher | Universidad Industrial de Santander | |
dc.publisher.faculty | Facultad de Ingenierías Fisicoquímicas | |
dc.publisher.program | Ingeniería Química | |
dc.publisher.school | Escuela de Ingeniería Química | |
dc.rights | http://creativecommons.org/licenses/by/4.0/ | |
dc.rights.accessrights | info:eu-repo/semantics/openAccess | |
dc.rights.creativecommons | Atribución-NoComercial-SinDerivadas 4.0 Internacional (CC BY-NC-ND 4.0) | |
dc.rights.license | Attribution-NonCommercial 4.0 International (CC BY-NC 4.0) | |
dc.rights.uri | http://creativecommons.org/licenses/by-nc/4.0 | |
dc.subject | Arenas Negras | |
dc.subject | Ilmenita | |
dc.subject | Concentración Gravimétrica | |
dc.subject | Separación Magnética | |
dc.subject | Molienda De Alta Energía | |
dc.subject | Nanométrico. | |
dc.subject.keyword | Black Sands | |
dc.subject.keyword | Ilmenite | |
dc.subject.keyword | Gravimetric Concentration | |
dc.subject.keyword | Magnetic Separation | |
dc.subject.keyword | High Energy Milling | |
dc.subject.keyword | Nanometric. | |
dc.title | Concentración de arenas negras provenientes de Barbacoas (Nariño) y evaluación de su procesamiento por molienda de alta energía para la obtención de ilmenita de tamaño nanométrico | |
dc.title.english | Black sands concentration from barbacoas (nariño) and evaluation of its processing by high energy milling for the obtainment of ilmenite of nanometric size | |
dc.type.coar | http://purl.org/coar/version/c_b1a7d7d4d402bcce | |
dc.type.hasversion | http://purl.org/coar/resource_type/c_7a1f | |
dc.type.local | Tesis/Trabajo de grado - Monografía - Pregrado |
Files
Original bundle
1 - 3 of 3
No Thumbnail Available
- Name:
- Carta de autorización.pdf
- Size:
- 676.63 KB
- Format:
- Adobe Portable Document Format
No Thumbnail Available
- Name:
- Nota de proyecto.pdf
- Size:
- 216.4 KB
- Format:
- Adobe Portable Document Format