Logotipo del repositorio

Publicación:
Obtencion y caracterizacion de elastometros de poliuretano a partir de aceite de higuerilla modificado

dc.contributor.advisorPulido Florez, Jorge Enrique
dc.contributor.advisorRamirez Garcia, Alvaro
dc.contributor.authorDuarte Leon, Diana Marcela
dc.contributor.authorValdivieso Gelves, Maria Lucia
dc.date.accessioned2024-03-03T04:35:59Z
dc.date.available2004
dc.date.available2024-03-03T04:35:59Z
dc.date.created2004
dc.date.issued2004
dc.description.abstractEn el presente trabajo se utilizó la reacción de transesterificación para modificar el aceite de higuerilla con glicerina y pentaeritritol con el propósito de aumentar la funcionalidad (índice de hidroxilo) de los polioles que fueron usados en la obtención de los poliuretanos. Se encontró que las condiciones para llevar a cabo la modificación con pentaeritritol y glicerina son: temperatura 210 °C, tiempo 2 horas y oxido de plomo (0,05%) como catalizador. Los polioles fueron caracterizados mediante la medición de viscosidad, índice de hidroxilo, pH, valor ácido, gravedad específica y espectroscopia de infrarrojo (IR). Los polioles obtenidos a partir de la modificación con pentaeritritol presentaron mayor índice de hidroxilo que los producidos con glicerina. Los elastómeros se obtuvieron mediante el método de pieza fundida líquida con una relación NCO/OH = 0,7 que permitió la preparación de los poliuretanos con los polioles escogidos y así comparar sus propiedades; el tiempo de curado fue de 4 horas a una temperatura de 100 °C. Los poliuretanos obtenidos a partir de aceite de higuerilla modificado con pentaeritritol presentaron mayor resistencia a la tensión, dureza shore A y resistencia al ataque químico en comparación con los poliuretanos producto del aceite de higuerilla puro y el aceite modificado con glicerina, lo cual muestra la marcada influencia del pentaeritritol en la estructura del poliol, la cual permite un mayor entrecruzamiento en la red de poliuretano. También se hicieron análisis termogravimetricos (TGAs) a todos los elastómeros obtenidos con el fin de caracterizarlos térmicamente.
dc.description.abstractenglishIn the present work the transesterification reaction was used to modify the castor oil with glycerin and pentaerythritol with the purpose to grow up the functionality (hydroxyl value) of the polyols that were used to obtain the polyurethanes. It was found that the conditions to carry out the modification with pentaerythritol and glycerin were: Temperature 210°C, time 2 h and litharge (0.05%) as catalyst; the polyols were characterized by the viscosity measurement, hydroxyl value, pH, acid value, specific gravity and infrared spectroscopy (IR), The obtained polyols from the modification with pentaerythritol had larger hydroxyl value than the polyols produced with glycerin. The polyurethane elastomers were obtained by casting method with a relation of NCO/OH = 0.7 that allowed the preparation of the polyurethanes from the chosen polyols and compare their properties; the time of curing was 4 hours at 100 °C of temperature. The obtained polyurethanes from the modified castor oil with pentaerythritol had larger tensile strength. Shore A hardness and chemical reagents resistance are also larger than the polyurethanes made from pure castor oil and also from modified castor oil with glycerin. This shows the notable influence of the pentaerythritol in the polyol structure, that allows a larger crosslinking in the polyurethane network. Thermogravimetrics analysis (TGA) were realized to all obtained elastomers in order to measure their thermal characterization
dc.description.degreelevelPregrado
dc.description.degreenameIngeniero Químico
dc.format.mimetypeapplication/pdf
dc.identifier.instnameUniversidad Industrial de Santander
dc.identifier.reponameUniversidad Industrial de Santander
dc.identifier.repourlhttps://noesis.uis.edu.co
dc.identifier.urihttps://noesis.uis.edu.co/handle/20.500.14071/16100
dc.language.isospa
dc.publisherUniversidad Industrial de Santander
dc.publisher.facultyFacultad de Ingenierías Fisicoquímicas
dc.publisher.programIngeniería Química
dc.publisher.schoolEscuela de Ingeniería Química
dc.rightshttp://creativecommons.org/licenses/by/4.0/
dc.rights.accessrightsinfo:eu-repo/semantics/openAccess
dc.rights.creativecommonsAtribución-NoComercial-SinDerivadas 4.0 Internacional (CC BY-NC-ND 4.0)
dc.rights.licenseAttribution-NonCommercial 4.0 International (CC BY-NC 4.0)
dc.rights.urihttp://creativecommons.org/licenses/by-nc/4.0
dc.subjectAceite de higuerilla
dc.subjectTransesterificación
dc.subjectPentaeritritol
dc.subjectElastómero.
dc.subject.keywordCastor oil
dc.subject.keywordTransesterification
dc.subject.keywordPentaerythritol
dc.subject.keywordPolyurethanes
dc.titleObtencion y caracterizacion de elastometros de poliuretano a partir de aceite de higuerilla modificado
dc.title.englishPreparation and characterization of modified castor oil polyurethane elastomers
dc.type.coarhttp://purl.org/coar/version/c_b1a7d7d4d402bcce
dc.type.hasversionhttp://purl.org/coar/resource_type/c_7a1f
dc.type.localTesis/Trabajo de grado - Monografía - Pregrado
dspace.entity.typePublication

Archivos

Bloque original

Mostrando 1 - 2 de 2
Cargando...
Miniatura
Nombre:
Documento.pdf
Tamaño:
2.81 MB
Formato:
Adobe Portable Document Format
Cargando...
Miniatura
Nombre:
Nota de proyecto.pdf
Tamaño:
583.8 KB
Formato:
Adobe Portable Document Format

VIGILADA MINEDUCACIÓN

Ordenanza No. 83 de 1.944 (junio 22)

Carácter académico: Universidad

Notificaciones judiciales: notjudiciales@uis.edu.co 

.

Código SNIES: 1204   Nit: 890.201.213-4

Línea Anticorrupción:  +57 (601) 562 9300 EXT: 3633

Línea transparente: +57 (607) 630 3031